Unravelling the origin of capacity fade in Prussian white hard carbon full cells through operando X-ray diffraction (2024)

Unravelling the origin of capacity fade in Prussian white hard carbon full cells through operando X-ray diffraction, Ida Nielsen, C. A. Hall, A-M. Mattsson, R. Younesi, A. Buckel, G. Ek, and W. R. Brant. J. Mater. Chem. A. 2024, 12, 17413-17421. https://doi.org/10.1039/D4TA02325K